Let us figure out the surface treatment of modern landscape stainless steel sculptures. The cleanliness of the metal surface used in the processing of stainless steel seriously affects the bonding force of the painted paint layer. If the residual or adsorbed water, oil and other matter on the surface of the workpiece are not cleaned, and pinholes and nodules are often generated. The separation of oil and water in the compressed air used for spraying is not complete enough, so that the compressed air contains excessive amounts of water and oil, which will inevitably affect the quality of the spray coating film layer of city Sculpture and cause various fault defects.
The construction tools that need to be used in the processing of stainless steel Corten steel sculptures are: air pump, gas filter tank, air duct and spray gun. According to the material features, after photostatting, the paint should be sprayed in time within 24 hours. The steel parts must be sprayed within six hours after sandblasting and shot peening. This Modern stainless steel sculpture processing method is a good way to improve the adhesion of the coating film to the substrate and enhance its corrosion resistance.
Therefore, it is necessary to insist on regularly cleaning Outdoor Sculptures and replacing the filtrate in the oil-water separation facility to keep the compressed air clean and clean, which is beneficial to improve the performance of the painted paint layer. Moreover, the influence of the temperature and humidity of the paint painting site on the quality of the spray coating film layer is very obvious.
It should be noted that the construction site temperature of the stainless steel sculpture processing should be in the range of 10 to 30 °C, and the relative humidity should not exceed 80%. The construction site must be kept clean, clean and orderly. The temperature is too high, the relative humidity is large, the painted paint layer is easy to be white, showing orange peel, etc., and when the temperature is too low, the paint layer is easy to flow, which has an adverse effect on the quality of the coated metal surface coating.